选区激光熔化AlSi10Mg-Er-Zr合金微观组织及力学性能强化 |
| 杨天野, 崔丽, 贺定勇, 黄晖 |
|
Enhancement of Microstructure and Mechanical Property of AlSi10Mg-Er-Zr Alloys Fabricated by Selective Laser Melting |
| YANG Tianye, CUI Li, HE Dingyong, HUANG Hui |
| 图5 SLM成形AlSi10Mg-Er-Zr及AlSi10Mg试样组织反极图及晶粒尺寸分布图 |
| Fig.5 Inverse pole figure maps of AlSi10Mg-Er-Zr (a) and AlSi10Mg (b) samples fabricated by SLM and grains size distribution of SLM sample (c) |
|