金属材料局部腐蚀损伤过程的近场动力学模拟:进展与挑战 |
| 夏大海, 邓成满, 陈子光, 李天书, 胡文彬 |
|
Modeling Localized Corrosion Propagation of Metallic Materials by Peridynamics: Progresses and Challenges |
| XIA Dahai, DENG Chengman, CHEN Ziguang, LI Tianshu, HU Wenbin |
| 图10 盐膜的形成、原PD模型和改进的PD模型得到的腐蚀损伤的时间演化[ |
| Fig.10 Formation of the effect of the salt layer (a), time-evolution of corrosion damage (see legend) with the earlier PD model (left side of the figure) and the newly proposed PD model (right side of the figure) (b)[ |
|