金属材料局部腐蚀损伤过程的近场动力学模拟:进展与挑战 |
| 夏大海, 邓成满, 陈子光, 李天书, 胡文彬 |
|
Modeling Localized Corrosion Propagation of Metallic Materials by Peridynamics: Progresses and Challenges |
| XIA Dahai, DENG Chengman, CHEN Ziguang, LI Tianshu, HU Wenbin |
| 图7 PD腐蚀模型预测结果和实验测得极化曲线的对比结果及“域因子”(m)收敛性研究[ |
| Fig.7 Comparison of polarization of PD model and experimental (a), and horizon factor (m)-convergence (b-d)[ |
|