制备工艺对FGH4097高温合金微观组织与性能的影响 |
| 解磊鹏, 孙文瑶, 陈明辉, 王金龙, 王福会 |
|
Effects of Processing on Microstructures and Properties of FGH4097 Superalloy |
| XIE Leipeng, SUN Wenyao, CHEN Minghui, WANG Jinlong, WANG Fuhui |
| 图7 HP和SPS方法制备的FGH4097合金在900℃下氧化100 h的动力学曲线及氧化速率曲线 |
| Fig.7 Isothermal oxidation kinetics of the FGH4097 alloys prepared by HP and SPS at 900oC for 100 h (y—oxidation weight gain per unit area, t—oxidation time, kp—rate constant of the parabola, y2 = kpt) (a) y vs t (b) y2vs t |
|