制备工艺对FGH4097高温合金微观组织与性能的影响 |
| 解磊鹏, 孙文瑶, 陈明辉, 王金龙, 王福会 |
|
Effects of Processing on Microstructures and Properties of FGH4097 Superalloy |
| XIE Leipeng, SUN Wenyao, CHEN Minghui, WANG Jinlong, WANG Fuhui |
| 图6 HP和SPS方法制备的FGH4097合金在25℃下拉伸后的断裂表面及断口形貌 |
| Fig.6 Fracture surface (a, b) and cross-sectional (c-f) morphologies of FGH4097 alloys prepared by HP (a, c, e) and SPS (b, d, f) after tensile test at 25oC (GB—grain boundary) |
|