TiAl合金板材轧制研究现状 |
| 陈玉勇, 叶园, 孙剑飞 |
|
Present Status for Rolling TiAl Alloy Sheet |
| CHEN Yuyong, YE Yuan, SUN Jianfei |
| 图13 铸锭直接热轧坯料宏观形貌[ |
| Fig.13 Appearance of direct-rolling billet[ (a) Ti-45Al-8.5Nb-0.2W-0.2B-0.2Y alloy billet (b) billet + soft can |
|