TiAl
合金板材轧制研究现状
陈玉勇, 叶园, 孙剑飞
Present Status for Rolling TiAl Alloy Sheet
CHEN Yuyong, YE Yuan, SUN Jianfei
图10
Ti-45Al-7Nb-0.3W合金板材(变形量73%)显微组织
[
28
]
Fig.10
Microstructure of Ti-45Al-7Nb-0.3W alloy sheet (reduction 73%)
[
28
]