TiAl
合金板材轧制研究现状
陈玉勇, 叶园, 孙剑飞
Present Status for Rolling TiAl Alloy Sheet
CHEN Yuyong, YE Yuan, SUN Jianfei
图9
粉末冶金轧制
γ
-TiAl合金板材
[
27
]
Fig.9
γ
-TiAl alloy sheet of PM rolling
[
27
]
(a) microstructure (b) appearance