TiAl合金板材轧制研究现状 |
| 陈玉勇, 叶园, 孙剑飞 |
|
Present Status for Rolling TiAl Alloy Sheet |
| CHEN Yuyong, YE Yuan, SUN Jianfei |
| 图5 Ti-44Al-8Nb-0.2W-0.2B-Y合金板材及轧制Ti-45Al-8.5Nb-(W, B, Y)合金显微组织[ |
| Fig.5 Microstructures of Ti-44Al-8Nb-0.2W-0.2B-Y alloy sheet (a-c)[ (a) low magnification (b) residual lamellar region (c) duplex microstructure region (d) normal direction section (e) RD section |
|