新型无机硅酸盐复合涂层制备及其在高温水蒸气环境的氧化行为 |
| 丛鸿达, 王金龙, 王成, 宁珅, 高若恒, 杜瑶, 陈明辉, 朱圣龙, 王福会 |
|
A New Design Inorganic Silicate Composite Coating and Its Oxidation Behavior at High Temperature in Steam Atmosphere |
| CONG Hongda, WANG Jinlong, WANG Cheng, NING Shen, GAO Ruoheng, DU Yao, CHEN Minghui, ZHU Shenglong, WANG Fuhui |
| 图3 CB2钢和无机防护涂层在水蒸气650℃高温环境中氧化1000 h后的XRD谱 |
| Fig.3 XRD spectra of CB2 steel (a) and its inorganic coating (b) after oxidized in high-temperature steam atmosphere at 650oC for 1000 h |
|