Pb-Al合金定向凝固组织形成过程 |
| 李彦强, 赵九洲, 江鸿翔, 何杰 |
|
Microstructure Formation in Directionally Solidified Pb-Al Alloy |
| LI Yanqiang, ZHAO Jiuzhou, JIANG Hongxiang, HE Jie |
| 图8 不同凝固速率下熔体温度、组元互溶温度及粒子形核率沿z轴的变化,以及凝固界面形状 |
| Fig.8 T, Ts of the matrix melt, and I of the Al-rich particles in front of the solidification interface along the central z-axes for the Pb-0.15Al alloys solidified at V0 = 4 mm/s (blue lines), 7 mm/s (red lines), and 10 mm/s (black lines) (The inset shows the shape of the solidification interface at different V0) |
|