Pb-Al合金定向凝固组织形成过程 |
| 李彦强, 赵九洲, 江鸿翔, 何杰 |
|
Microstructure Formation in Directionally Solidified Pb-Al Alloy |
| LI Yanqiang, ZHAO Jiuzhou, JIANG Hongxiang, HE Jie |
| 图5 Pb-0.15Al合金中富Al粒子的二维平均半径(<R>2D)随凝固速率的变化 |
| Fig.5 Average 2D radius (<R>2D) of the Al-rich particles in the Pb-0.15Al alloys directionally solidified at different V0 |
|