Y元素对Cu-Al-Ni高温形状记忆合金性能的影响 |
| 张鑫, 崔博, 孙斌, 赵旭, 张欣, 刘庆锁, 董治中 |
|
Effect of Y Element on the Properties of Cu-Al-Ni High Temperature Shape Memory Alloy |
| ZHANG Xin, CUI Bo, SUN Bin, ZHAO Xu, ZHANG Xin, LIU Qingsuo, DONG Zhizhong |
| 图6 Cu-13Al-4Ni-xY (x = 0、0.2、0.5)合金在3.5%NaCl溶液中的动电位极化曲线 |
| Fig.6 Potential polarization curves for the Cu-13Al-4Ni-xY (x = 0, 0.2, 0.5) alloys in the 3.5%NaCl solution |
|