Y元素对Cu-Al-Ni高温形状记忆合金性能的影响 |
| 张鑫, 崔博, 孙斌, 赵旭, 张欣, 刘庆锁, 董治中 |
|
Effect of Y Element on the Properties of Cu-Al-Ni High Temperature Shape Memory Alloy |
| ZHANG Xin, CUI Bo, SUN Bin, ZHAO Xu, ZHANG Xin, LIU Qingsuo, DONG Zhizhong |
| 图2 Cu-13Al-4Ni-xY (x = 0.2、0.5)合金的XRD谱 |
| Fig.2 XRD spectra of Cu-13Al-4Ni-xY (x = 0.2 and 0.5) alloys |
|