CrMoTi中熵合金的性能及其原位合金化增材制造 |
| 刘广, 陈鹏, 姚锡禹, 陈朴, 刘星辰, 刘朝阳, 严明 |
|
Properties of CrMoTi Medimum-Entropy Alloy and Its In Situ Alloying Additive Manufacturing |
| LIU Guang, CHEN Peng, YAO Xiyu, CHEN Pu, LIU Xingchen, LIU Chaoyang, YAN Ming |
| 图11 增材制造原位合金化DLD1350W和SLM167J样品的SEM像和EDS分析 |
| Fig.11 SEM image and corresponding EDS results of samples DLD1350W (a) and SLM167J (b) (DLD1350W denotes the DLDed sample fabricated using P = 1350 W; SLM167J denotes the SLMed sample fabricated with VED = 167 J/mm3) |
|