CrMoTi中熵合金的性能及其原位合金化增材制造 |
| 刘广, 陈鹏, 姚锡禹, 陈朴, 刘星辰, 刘朝阳, 严明 |
|
Properties of CrMoTi Medimum-Entropy Alloy and Its In Situ Alloying Additive Manufacturing |
| LIU Guang, CHEN Peng, YAO Xiyu, CHEN Pu, LIU Xingchen, LIU Chaoyang, YAN Ming |
| 图8 SLM加工CrMoTi中熵合金试样截面形貌的SEM像 |
| Fig.8 Cross-section SEM image of SLMed CrMoTi MEA |
|