CrMoTi中熵合金的性能及其原位合金化增材制造 |
| 刘广, 陈鹏, 姚锡禹, 陈朴, 刘星辰, 刘朝阳, 严明 |
|
Properties of CrMoTi Medimum-Entropy Alloy and Its In Situ Alloying Additive Manufacturing |
| LIU Guang, CHEN Peng, YAO Xiyu, CHEN Pu, LIU Xingchen, LIU Chaoyang, YAN Ming |
| 图7 增材制造原位合金化CrMoTi中熵合金成型效果 |
| Fig.7 Top-views (a1, b1) and side-views (a2, b2) of CrMoTi MEA fabricated by DLD (a1, a2) and SLM (b1, b2) in situ alloying |
|