CrMoTi中熵合金的性能及其原位合金化增材制造 |
| 刘广, 陈鹏, 姚锡禹, 陈朴, 刘星辰, 刘朝阳, 严明 |
|
Properties of CrMoTi Medimum-Entropy Alloy and Its In Situ Alloying Additive Manufacturing |
| LIU Guang, CHEN Peng, YAO Xiyu, CHEN Pu, LIU Xingchen, LIU Chaoyang, YAN Ming |
| 图3 通过电弧熔炼、DLD和选区激光熔化(SLM)成型的CrMoTi中熵合金XRD谱 |
| Fig.3 XRD spectra of CrMoTi medium-entropy alloys (MEA) fabricated by arc melting, DLD, and selective laser melting (SLM) techniques |
|