CrMoTi中熵合金的性能及其原位合金化增材制造 |
| 刘广, 陈鹏, 姚锡禹, 陈朴, 刘星辰, 刘朝阳, 严明 |
|
Properties of CrMoTi Medimum-Entropy Alloy and Its In Situ Alloying Additive Manufacturing |
| LIU Guang, CHEN Peng, YAO Xiyu, CHEN Pu, LIU Xingchen, LIU Chaoyang, YAN Ming |
| 图1 直接激光沉积(DLD)使用的混合元素粉末的SEM-EDS像 |
| Fig.1 SEM-EDS image of the blended elemental powder used for direct laser deposition (DLD) |
|