粗糙表面高强铝合金导线疲劳寿命预测 |
| 宋文硕, 宋竹满, 罗雪梅, 张广平, 张滨 |
|
Fatigue Life Prediction of High Strength Aluminum Alloy Conductor Wires with Rough Surface |
| SONG Wenshuo, SONG Zhuman, LUO Xuemei, ZHANG Guangping, ZHANG Bin |
| 图7 不同表面粗糙度对应的疲劳断口扩展区面积 |
| Fig.7 Fatigue fracture expansion areas corresponding to different roughnesses (The yellow areas are expansion areas, and green areas are instantaneous fracture areas) |
|