粗糙表面高强铝合金导线疲劳寿命预测 |
| 宋文硕, 宋竹满, 罗雪梅, 张广平, 张滨 |
|
Fatigue Life Prediction of High Strength Aluminum Alloy Conductor Wires with Rough Surface |
| SONG Wenshuo, SONG Zhuman, LUO Xuemei, ZHANG Guangping, ZHANG Bin |
| 图6 不同粗糙度6061铝合金导线样品的应力幅-粗糙度关系和断口形貌 |
| Fig.6 Relationship of stress amplitude and Rz and corresponding fracture morphologies (insets) of 6061 aluminum alloy conductor wire specimens with different roughnesses (a) 104~105 cyc (b) 105~106 cyc |
|