粗糙表面高强铝合金导线疲劳寿命预测 |
| 宋文硕, 宋竹满, 罗雪梅, 张广平, 张滨 |
|
Fatigue Life Prediction of High Strength Aluminum Alloy Conductor Wires with Rough Surface |
| SONG Wenshuo, SONG Zhuman, LUO Xuemei, ZHANG Guangping, ZHANG Bin |
| 图4 不同表面粗糙度6061铝合金导线样品的应力幅-疲劳寿命(S-N)曲线 |
| Fig.4 Stress amplitude-fatigue life (S-N) curves of 6061 aluminum alloy conductor wire specimens with different surface roughness (The arrow indicates that the sample is not failure under this stress amplitude and cycle) |
|