粗糙表面高强铝合金导线疲劳寿命预测 |
| 宋文硕, 宋竹满, 罗雪梅, 张广平, 张滨 |
|
Fatigue Life Prediction of High Strength Aluminum Alloy Conductor Wires with Rough Surface |
| SONG Wenshuo, SONG Zhuman, LUO Xuemei, ZHANG Guangping, ZHANG Bin |
| 图1 疲劳样品尺寸示意图 |
| Fig.1 Schematic of specimen dimension for fatigue testing (Ra—arithmetical mean deviation of the profile; unit: mm) |
|