冷速对高碳铬轴承钢液析碳化物凝固析出机制的影响 |
| 李闪闪, 陈云, 巩桐兆, 陈星秋, 傅排先, 李殿中 |
|
Effect of Cooling Rate on the Precipitation Mechanism of Primary Carbide During Solidification in High Carbon-Chromium Bearing Steel |
| LI Shanshan, CHEN Yun, GONG Tongzhao, CHEN Xingqiu, FU Paixian, LI Dianzhong |
| 图9 电解萃取GCr15SiMn和GCr15SiMn(RE)连铸轴承钢锭液析碳化物颗粒的SEM像和XRD谱 |
| Fig.9 SEM images (a, b) and XRD spectra (c, d) of primary carbides obtained by electrolytic extraction in GCr15SiMn (a, c) and GCr15SiMn(RE) (b, d) steels |
|