冷速对高碳铬轴承钢液析碳化物凝固析出机制的影响 |
| 李闪闪, 陈云, 巩桐兆, 陈星秋, 傅排先, 李殿中 |
|
Effect of Cooling Rate on the Precipitation Mechanism of Primary Carbide During Solidification in High Carbon-Chromium Bearing Steel |
| LI Shanshan, CHEN Yun, GONG Tongzhao, CHEN Xingqiu, FU Paixian, LI Dianzhong |
| 图3 试样熔化和凝固实验过程中的加热和冷却曲线 |
| Fig.3 Heating and cooling curves of the sample in the remelting and solidification experiments |
|