高温低周疲劳下C-HRA-5奥氏体耐热钢中孪晶界演变 |
| 周红伟, 高建兵, 沈加明, 赵伟, 白凤梅, 何宜柱 |
|
Twin Boundary Evolution Under Low-Cycle Fatigue of C-HRA-5 Austenitic Heat-Resistant Steel at High Temperature |
| ZHOU Hongwei, GAO Jianbing, SHEN Jiaming, ZHAO Wei, BAI Fengmei, HE Yizhu |
| 图10 C-5钢中疲劳裂纹与残留TBs的EBSD分析 |