700℃热暴露对 β 凝固 γ-TiAl合金表面组织及形貌的影响 |
| 刘仁慈, 王鹏, 曹如心, 倪明杰, 刘冬, 崔玉友, 杨锐 |
|
Influence of Thermal Exposure at 700oC on the Microstructure and Morphology in the Surface of β-Solidifying γ-TiAl Alloys |
| LIU Renci, WANG Peng, CAO Ruxin, NI Mingjie, LIU Dong, CUI Yuyou, YANG Rui |
| 图8 热暴露过程中表面反应界面显微组织、成分及形貌演变机理 |
| Fig.8 Evolution mechanism of microstructure, composition distribution, and morphology near the reaction interface of TNM-0.5B alloy during thermal exposure for 0 h (a), 10 h (b), 100 h (c), 200 h (d), and 500 h (e) |
|