700℃热暴露对 β 凝固 γ-TiAl合金表面组织及形貌的影响 |
| 刘仁慈, 王鹏, 曹如心, 倪明杰, 刘冬, 崔玉友, 杨锐 |
|
Influence of Thermal Exposure at 700oC on the Microstructure and Morphology in the Surface of β-Solidifying γ-TiAl Alloys |
| LIU Renci, WANG Peng, CAO Ruxin, NI Mingjie, LIU Dong, CUI Yuyou, YANG Rui |
| 图7 热暴露样品反应界面显微组织BSE像及元素分布图 |
| Fig.7 BSE images of microstructures near the reaction interface of samples thermal exposed for 10 h (a), 100 h (b), and 500 h (c), and element distributions of Al (d), Ti (e), O (f), N (g), Mo (h), and Nb (i) near the interface of sample thermal exposed for 500 h (Main elements in specific layer of oxidation were summarized in the right of Fig.7f; rectangulars in Fig.7d, e, h, and i show the main elements distributions near the reaction interface of β0 phase) |
|