700℃热暴露对 β 凝固 γ-TiAl合金表面组织及形貌的影响 |
| 刘仁慈, 王鹏, 曹如心, 倪明杰, 刘冬, 崔玉友, 杨锐 |
|
Influence of Thermal Exposure at 700oC on the Microstructure and Morphology in the Surface of β-Solidifying γ-TiAl Alloys |
| LIU Renci, WANG Peng, CAO Ruxin, NI Mingjie, LIU Dong, CUI Yuyou, YANG Rui |
| 图6 700℃热暴露不同时间样品表面纵切面显微组织的OM像 |
| Fig.6 OM images of microstructures in the surface of samples thermal exposed at 700oC in air for 10 h (a), 100 h (b), 200 h (c), and 500 h (d) (Insets in Fig.6b show the γ and β0 phase layer characteristics of oxidation front, respectively) |
|