700℃热暴露对 β 凝固 γ-TiAl合金表面组织及形貌的影响 |
| 刘仁慈, 王鹏, 曹如心, 倪明杰, 刘冬, 崔玉友, 杨锐 |
|
Influence of Thermal Exposure at 700oC on the Microstructure and Morphology in the Surface of β-Solidifying γ-TiAl Alloys |
| LIU Renci, WANG Peng, CAO Ruxin, NI Mingjie, LIU Dong, CUI Yuyou, YANG Rui |
| 图4 700℃热暴露不同时间样品表面三维轮廓 |
| Fig.4 Surface profiles of samples thermal exposed at 700oC in air for 0 h (a), 100 h (b), 200 h (c), and 500 h (d) |
|