纳入残余应力时不同拘束下DMWJ的断裂行为 |
| 吴进, 杨杰, 陈浩峰 |
|
Fracture Behavior of DMWJ Under Different Constraints Considering Residual Stress |
| WU Jin, YANG Jie, CHEN Haofeng |
| 图8 上下两面加载时a / W = 0.2和0.7拘束SENB试样的J-R曲线 |