辐照条件下Fe-Cu合金中富Cu析出相的临界形核尺寸和最小能量路径的弦方法计算 |
|||||||||||||||
| 刘续希, 柳文波, 李博岩, 贺新福, 杨朝曦, 恽迪 | |||||||||||||||
|
Calculation of Critical Nucleus Size and Minimum Energy Path of Cu-Riched Precipitates During Radiation in Fe-Cu Alloy Using String Method |
|||||||||||||||
| LIU Xuxi, LIU Wenbo, LI Boyan, HE Xinfu, YANG Zhaoxi, YUN Di | |||||||||||||||
| 表5 650 K下演化50步后不同Fe-Cu合金的临界团簇半径与平均浓度计算结果 |
|||||||||||||||
| Table 5 Calculation results of RC and CC for different Fe-Cu alloys at 650 K after 50-step-revolution |
|||||||||||||||
|
|||||||||||||||