| 刘续希, 柳文波, 李博岩, 贺新福, 杨朝曦, 恽迪 |
|
Calculation of Critical Nucleus Size and Minimum Energy Path of Cu-Riched Precipitates During Radiation in Fe-Cu Alloy Using String Method |
| LIU Xuxi, LIU Wenbo, LI Boyan, HE Xinfu, YANG Zhaoxi, YUN Di |
| 图8 650 K下演化50步后不同Cu元素元素浓度Fe-Cu合金临界团簇的Cu元素浓度分布和团簇形貌 |
| Fig.8 Cu concentration distributions and top views of cluster morphologies of critical nucleus (insets) of Fe-Cu alloy after 50-step-revolution with Cu concentrations of 0.05% (a), 0.1% (b), 0.3% (c), and 0.5% (d) at 650 K |
|