辐照条件下Fe-Cu合金中富Cu析出相的临界形核尺寸和最小能量路径的弦方法计算 |
| 刘续希, 柳文波, 李博岩, 贺新福, 杨朝曦, 恽迪 |
|
Calculation of Critical Nucleus Size and Minimum Energy Path of Cu-Riched Precipitates During Radiation in Fe-Cu Alloy Using String Method |
| LIU Xuxi, LIU Wenbo, LI Boyan, HE Xinfu, YANG Zhaoxi, YUN Di |
| 图5 不同温度下演化50步后Fe-0.3%Cu合金临界团簇的Cu元素浓度分布和团簇形貌 |
| Fig.5 Cu concentration distributions and top views of cluster morphologies of critical nucleus (insets) of Fe-0.3%Cu alloy after 50-step-revolution at 550 K (a), 600 K (b), 650 K (c), and 700 K (d) |
|