辐照条件下Fe-Cu合金中富Cu析出相的临界形核尺寸和最小能量路径的弦方法计算 |
| 刘续希, 柳文波, 李博岩, 贺新福, 杨朝曦, 恽迪 |
|
Calculation of Critical Nucleus Size and Minimum Energy Path of Cu-Riched Precipitates During Radiation in Fe-Cu Alloy Using String Method |
| LIU Xuxi, LIU Wenbo, LI Boyan, HE Xinfu, YANG Zhaoxi, YUN Di |
| 图1 形核过程鞍点示意图 |
| Fig.1 Schematics of saddle points in the nucleus evolutionary correction process (a) energy path saddle point diagram(b) energy path height contrast diagram |
|