喷射成形AlSiCuMg合金的热变形组织演变及再结晶行为 |
| 吴彩虹, 冯迪, 臧千昊, 范诗春, 张豪, 李胤樹 |
|
Microstructure Evolution and Recrystallization Behavior During Hot Deformation of Spray Formed AlSiCuMg Alloy |
| WU Caihong, FENG Di, ZANG Qianhao, FAN Shichun, ZHANG Hao, LEE Yunsoo |
| 图7 不同变形条件下喷射成形Al25Si4Cu1Mg合金的热变形组织演变示意图 |
| Fig.7 Schematics of hot deformation microstructure evolution of spray formed Al25Si4Cu1Mg alloy under different deformation conditions (Z—Zener-Hollomon parameter) |
|