喷射成形AlSiCuMg合金的热变形组织演变及再结晶行为 |
| 吴彩虹, 冯迪, 臧千昊, 范诗春, 张豪, 李胤樹 |
|
Microstructure Evolution and Recrystallization Behavior During Hot Deformation of Spray Formed AlSiCuMg Alloy |
| WU Caihong, FENG Di, ZANG Qianhao, FAN Shichun, ZHANG Hao, LEE Yunsoo |
| 图5 Al25Si4Cu1Mg喷射态和不同热压缩条件下的晶粒组织形貌EBSD像 |
| Fig.5 EBSD images of as-sprayed and deformed microstructures under different hot compressed conditions of Al25Si4Cu1Mg alloy (The grain boundaries colored by red indicate the misorientation in the range of 2°-15°. The grain boundaries colored by black indicate the misorientation > 15°) (a) as-sprayed (b) Td = 623 K, (d) Td = 673 K, |
|