表1 方程组(2)中的常数p1~p8和q1~q10参数值
Table 1 Parameter values of constants p1-p8 and q1-q10 in Eq.(2)
ipiqi
1-0.257542097245903-294046.970408271
2-2.83015706572016178976.497962565
32.45922736413675-69271.2661368186
4-0.36379389490468810360.1236350591
5-16.26920605468641550446.7040738
60.283900116701206-3206585.50013
70.010848953995002429.3705896768819
8118.828514840866-30.9026912200925
9423.402071622377
10-1786.70014340018