砂型3DP打印参数对ZL205A合金铸造性能的影响 |
| 王春辉, 杨光昱, 阿热达克·阿力玛斯, 李晓刚, 介万奇 |
|
Effect of Printing Parameters of 3DP Sand Mold on the Casting Performance of ZL205A Alloy |
| WANG Chunhui, YANG Guangyu, ALIMASI Aredake, LI Xiaogang, JIE Wanqi |
| 图3 不同树脂含量和打印层厚下3DP砂型制备的ZL205A合金热裂试棒宏观形貌 |
| Fig.3 Macro-morphologies of ZL205A alloy hot tearing susceptibility bars prepared by 3DP sand mold with different resin contents (mass fraction) and printing layer thicknesses (Hot crackings are marked by rectangles) |
|