砂型3DP打印参数对ZL205A合金铸造性能的影响 |
| 王春辉, 杨光昱, 阿热达克·阿力玛斯, 李晓刚, 介万奇 |
|
Effect of Printing Parameters of 3DP Sand Mold on the Casting Performance of ZL205A Alloy |
| WANG Chunhui, YANG Guangyu, ALIMASI Aredake, LI Xiaogang, JIE Wanqi |
| 图1 热裂倾向性测试和单螺旋流动性测试3DP砂型及其示意图 |
| Fig.1 Three-dimensional printing (3DP) sand mold (a) and schematics of hot tearing susceptibility testing (unit: mm) (b), and 3DP sand mold of the single-helix fluidity testing (c) |
|