应变工程中Bi(111)薄膜的半导体-半金属转变及其机理 |
| 任师浩, 刘永利, 孟凡顺, 祁阳 |
|
Strain-Engineered Semiconductor to Semimetallic Transition and Its Mechanism in Bi(111) Film |
| REN Shihao, LIU Yongli, MENG Fanshun, QI Yang |
| 图4 1 BL厚Bi(111)薄膜在不同应变下的能带结构 |
| Fig.4 Electronic band structures of 1 BL thickness Bi(111) film with different strains |
|