290℃氩离子辐照对Fe-Cu合金微观组织的影响 |
||||||||||||||||
| 朱小绘, 刘向兵, 王润中, 李远飞, 刘文庆 | ||||||||||||||||
|
Effects of Ar Ion Irradiation on Microstructure of Fe-Cu Alloys at 290oC |
||||||||||||||||
| ZHU Xiaohui, LIU Xiangbing, WANG Runzhong, LI Yuanfei, LIU Wenqing | ||||||||||||||||
| 表1 距表面不同深度处富Cu团簇等效半径、数量密度及基体中的Cu含量 |
||||||||||||||||
| Table 1 Average radii (Rp) and number densities (Nv) of Cu clusters at different depths and corresponding Cu concentrations in matrix (CCu, atomic fraction) |
||||||||||||||||
|
||||||||||||||||