290℃氩离子辐照对Fe-Cu合金微观组织的影响 |
| 朱小绘, 刘向兵, 王润中, 李远飞, 刘文庆 |
|
Effects of Ar Ion Irradiation on Microstructure of Fe-Cu Alloys at 290oC |
| ZHU Xiaohui, LIU Xiangbing, WANG Runzhong, LI Yuanfei, LIU Wenqing |
| 图1 氩离子辐照后Fe-Cu合金深度方向损伤剂量和离子浓度分布(SRIM 2008软件) |
| Fig.1 Distributions of damage dose and ion concentration (atomic fraction) of Ar ion irradiated Fe-Cu alloys as a function of depth (calculated by SRIM 2008) |
|