Ca、Mg掺杂下夹杂物对C70S6非调质钢点蚀行为的影响
孙阳庭, 李一唯, 吴文博, 蒋益明, 李劲

Effect of Inclusions on Pitting Corrosion of C70S6 Non-Quenched and Tempered Steel Doped with Ca and Mg
SUN Yangting, LI Yiwei, WU Wenbo, JIANG Yiming, LI Jin
表2 C70S6-CaMg非调质钢中夹杂物类型、数量及尺寸分布
Table 2 Inclusion type, number, and size of C70S6-CaMg non-quenched and tempered steel
Inclusion typeNumber0-2 μm2-5 μm5-10 μm> 10 μm
MnS677449491777480
MgO-MnS62392210
CaO-MnS32100
Al2O3-MnS2071426230
Spinel-MnS2301616720
Aluminate-MnS445299136100
Others49311710
Total777056232082650