Ca、Mg掺杂下夹杂物对C70S6非调质钢点蚀行为的影响
孙阳庭, 李一唯, 吴文博, 蒋益明, 李劲

Effect of Inclusions on Pitting Corrosion of C70S6 Non-Quenched and Tempered Steel Doped with Ca and Mg
SUN Yangting, LI Yiwei, WU Wenbo, JIANG Yiming, LI Jin
表1 C70S6非调质钢中夹杂物类型、数量及尺寸分布
Table 1 Inclusion type, number, and size of C70S6 non-quenched and tempered steel
Inclusion typeNumber0-2 μm2-5 μm5-10 μm> 10 μm
MnS4750248720641981
MgO-MnS127320
CaO-MnS1810800
Al2O3-MnS105633570
Spinel-MnS77344030
Aluminate-MnS1576876130
Others2311840
Total5142268022342271