Ca、Mg掺杂下夹杂物对C70S6非调质钢点蚀行为的影响
孙阳庭, 李一唯, 吴文博, 蒋益明, 李劲

Effect of Inclusions on Pitting Corrosion of C70S6 Non-Quenched and Tempered Steel Doped with Ca and Mg
SUN Yangting, LI Yiwei, WU Wenbo, JIANG Yiming, LI Jin
图2 C70S6夹杂形貌夹杂物的微观形貌及EDS元素分布图
Fig.2 Inclusion morphology (a) and element distribution maps (b) of C70S6