MoNb改性FeCrAl不锈钢高温组织演变和力学性能 |
| 温冬辉, 姜贝贝, 王清, 李相伟, 张鹏, 张书彦 |
|
Microstructure Evolution at Elevated Temperature and Mechanical Properties of MoNb-Modified FeCrAl Stainless Steel |
| WEN Donghui, JIANG Beibei, WANG Qing, LI Xiangwei, ZHANG Peng, ZHANG Shuyan |
| 图3 C35MN合金在800℃时效不同时间后微观组织的SEM像以及Laves相体积分数和尺寸变化曲线 |
| Fig.3 SEM images of the C35MN alloy aged at 800oC for 2 h (a), 8 h (b), 50 h (c), 100 h (d), 200 h (e), 300 h (f), and 400 h (g), and the corresponding variation curves of the volume fraction and precipitate size of Laves phase (h) |
|