MoNb改性FeCrAl不锈钢高温组织演变和力学性能 |
| 温冬辉, 姜贝贝, 王清, 李相伟, 张鹏, 张书彦 |
|
Microstructure Evolution at Elevated Temperature and Mechanical Properties of MoNb-Modified FeCrAl Stainless Steel |
| WEN Donghui, JIANG Beibei, WANG Qing, LI Xiangwei, ZHANG Peng, ZHANG Shuyan |
| 图1 C35MN合金经过800℃、24 h时效处理后微观组织的OM和SEM像 |
| Fig.1 OM (a) and SEM (b) images of the 800oC, 24 h aged C35MN alloy |
|