镍基高温合金K417G与氧化物耐火材料的界面反应 |
| 宋庆忠, 潜坤, 舒磊, 陈波, 马颖澈, 刘奎 |
|
Interfacial Reaction Between Nickel-Based Superalloy K417G and Oxide Refractories |
| SONG Qingzhong, QIAN Kun, SHU Lei, CHEN Bo, MA Yingche, LIU Kui |
| 图7 CaO熔炼的镍基高温合金K417G宏观形貌 |
| Fig.7 Macromorphology of nickel-based superalloy K417G smelted by CaO crucible |
|