镍基高温合金K417G与氧化物耐火材料的界面反应 |
| 宋庆忠, 潜坤, 舒磊, 陈波, 马颖澈, 刘奎 |
|
Interfacial Reaction Between Nickel-Based Superalloy K417G and Oxide Refractories |
| SONG Qingzhong, QIAN Kun, SHU Lei, CHEN Bo, MA Yingche, LIU Kui |
| 图6 CaO坩埚与镍基高温合金K417G界面的SEM像及EDS元素分布图 |
| Fig.6 SEM image (a) and EDS mappings (b-f) of the interface between CaO crucible and nickel-based superalloy K417G |
|